Bioresource Technology 2015-11-01

Understanding of pH value and its effect on autohydrolysis pretreatment prior to poplar chemi-thermomechanical pulping.

Lihui Liu, Wei Liu, Qingxi Hou, Junwei Chen, Ningpan Xu

Index: Bioresour. Technol. 196 , 662-7, (2015)

Full Text: HTML

Abstract

Autohydrolysis pretreatment with different severity factors was performed on poplar chips prior to chemi-thermomechanical pulping (CTMP) in order to investigate the change in pH value and its effect on the autohydrolysis pretreatment. The results showed that the dissolution amount of acetic acid increased with raising the severity factor of the pretreatment and declining the size of poplar chips, respectively. Besides, a logarithmic relationship between the amount of acetic acid released in the autohydrolysis liquor (AHL) and pH value of the AHL was observed. The amounts of glucose and xylose (including those in the form of monomers, oligomers, and polysaccharides) as well as furfural and hydroxymethylfurfural (HMF) also depended on the pH value of the AHL to some extent.Copyright © 2015 Elsevier Ltd. All rights reserved.

Related Compounds

Structure Name/CAS No. Articles
Sulfuric acid Structure Sulfuric acid
CAS:7664-93-9
D-(+)-Xylose Structure D-(+)-Xylose
CAS:58-86-6
acetic acid Structure acetic acid
CAS:1173022-32-6
acetic acid Structure acetic acid
CAS:64-19-7
Stanolone Structure Stanolone
CAS:521-18-6