Environmental Monitoring and Assessment 2014-10-01

Degradation of polyethylene by Trichoderma harzianum--SEM, FTIR, and NMR analyses.

H V Sowmya, Ramalingappa, M Krishnappa, B Thippeswamy

Index: Environ. Monit. Assess. 186(10) , 6577-86, (2014)

Full Text: HTML

Abstract

Trichoderma harzianum was isolated from local dumpsites of Shivamogga District for use in the biodegradation of polyethylene. Soil sample of that dumpsite was used for isolation of T. harzianum. Degradation was carried out using autoclaved, UV-treated, and surface-sterilized polyethylene. Degradation was monitored by observing weight loss and changes in physical structure by scanning electron microscopy, Fourier transform infrared spectroscopy, and nuclear magnetic resonance spectroscopy. T. harzianum was able to degrade treated polyethylene (40%) more efficiently than autoclaved (23%) and surface-sterilized polyethylene (13%). Enzymes responsible for polyethylene degradation were screened from T. harzianum and were identified as laccase and manganese peroxidase. These enzymes were produced in large amount, and their activity was calculated using spectrophotometric method and crude extraction of enzymes was carried out. Molecular weight of laccase was determined as 88 kDa and that of manganese peroxidase was 55 kDa. The capacity of crude enzymes to degrade polyethylene was also determined. By observing these results, we can conclude that this organism may act as solution for the problem caused by polyethylene in nature.


Related Compounds

Related Articles:

Long-term hip simulator testing of the artificial hip joint bearing surface grafted with biocompatible phospholipid polymer.

2014-03-01

[J. Orthop. Res. 32(3) , 369-76, (2014)]

Ultrasound assisted dialysis of semi-permeable membrane devices for the simultaneous analysis of a wide number of persistent organic pollutants.

2013-09-30

[Talanta 114 , 32-7, (2013)]

Hybrid composite membranes based on polyethylene separator and Al2O3 nanoparticles for lithium-ion batteries.

2013-05-01

[J. Nanosci. Nanotechnol. 13(5) , 3705-10, (2013)]

Polyethylene wear and osteolysis after cementless total hip arthroplasty with alumina-on-highly cross-linked polyethylene bearings in patients younger than thirty years of age.

2013-06-19

[J. Bone Joint Surg. Am. 95(12) , 1088-93, (2013)]

Application of nano-TiO2/LDPE composite film on photocatalytic oxidation degradation of dichloromethane.

2012-09-01

[J. Environ Biol. 33(5) , 955-9, (2012)]

More Articles...