Poly-4-Dioxan-2-One structure
|
Common Name | Poly-4-Dioxan-2-One | ||
---|---|---|---|---|
CAS Number | 29223-92-5 | Molecular Weight | 102.09 | |
Density | 1.201g/cm3 | Boiling Point | 222.895°C at 760 mmHg | |
Molecular Formula | C4H6O3 | Melting Point | 114°C | |
MSDS | USA | Flash Point | 85.464°C |
Name | Poly-4-Dioxan-2-One |
---|---|
Synonym | More Synonyms |
Density | 1.201g/cm3 |
---|---|
Boiling Point | 222.895°C at 760 mmHg |
Melting Point | 114°C |
Molecular Formula | C4H6O3 |
Molecular Weight | 102.09 |
Flash Point | 85.464°C |
Exact Mass | 102.032 |
Appearance of Characters | powder |
Storage condition | 20°C |
RIDADR | NONH for all modes of transport |
---|---|
WGK Germany | 3 |
A biomechanical study of laparoscopic 4S-modified Roeder and Weston knot strength in 3-0 polyglactin 910 and 3-0 polydioxanone.
Vet. Surg. 42(2) , 198-204, (2013) To (1) evaluate biomechanical strength of 4 different laparoscopic knots using 2 suture types, and (2) evaluate carotid artery ligature bursting pressure of 2 knots using a single suture type.Biomecha... |
|
In vitro analysis of polymer candidates for the development of absorbable vascular filters.
J. Vasc. Interv. Radiol. 23(8) , 1023-30, (2012) To test absorbable materials as a prelude to development of an absorbable vena cava filter for the prevention of pulmonary embolism (PE).Three absorbing polymer candidates, poliglecaprone (Monocryl; s... |
|
Generation of osteogenic construct using periosteal-derived osteoblasts and polydioxanone/pluronic F127 scaffold with periosteal-derived CD146 positive endothelial-like cells.
J. Biomed. Mater. Res. A 101(4) , 942-53, (2013) The purpose of this study was to generate tissue-engineered bone using human periosteal-derived osteoblasts (PO) and polydioxanone/pluronic F127 (PDO/pluronic F127) scaffold with preseeded human perio... |
MFCD00215855 |
1,4-Dioxan-2-one |