The use of styrene butadiene rubber (SBR) in tire rubber presents a challenge for the recycling of tire rubber because of its complex degradation behavior compared with that of natural rubber (NR). The effect of the composition of SBR on the degradation of NR was observed by light pyrolysis at variable times at 300 °C. The morphology, sol-gel evolution of the NR/SBR blends and the degradation mechanism was investigated. In addition, the structural evolution of the sol and gel fractions were measured by Fourier transform infrared spectroscopy (FTIR) and thermogravimetric analysis (TGA). The results indicated that the mechanism of degradation between SBR and NR differed significantly at 300 °C. The broken molecular chains present in SBR recombined with themselves or those of NR to form a new crosslinked network. The results also showed that the ratio of NR/SBR in the sol and gel fractions remains almost constant and unrelated to the original ratio of the NR/SBR blends. Following an increase in SBR content, the sol fraction of different NR/SBR blends mainly consisted of the small molecular chains of NR, whereas the gel fraction mostly constituted re-crosslinked SBR molecular chains.

Latest Articles:

Kinetics, evolving thermal properties, and surface ignition of carbon fiber reinforced epoxy composite during laser-induced decomposition

2018-04-11

[10.1016/j.polymdegradstab.2018.04.007]

Isolation and role of polylactic acid-degrading bacteria on degrading enzymes productions and PLA biodegradability at mesophilic conditions

2018-04-03

[10.1016/j.polymdegradstab.2018.03.023]

Rheological properties, oxidative and thermal stability, and potential application of biopolyols prepared via two-step process from crude glycerol

2018-03-28

[10.1016/j.polymdegradstab.2018.03.022]

Growth associated degradation of aliphatic-aromatic copolyesters by Cryptococcus sp. MTCC 5455

2018-03-27

[10.1016/j.polymdegradstab.2018.03.021]

Halloysite nanotubes and thymol as photo protectors of biobased polyamide 11

2018-03-27

[10.1016/j.polymdegradstab.2018.03.015]

More Articles...