... Please enable JavaScript to use all the features on this page. Journal of Catalysis. Volume 299, March 2013, Pages 20–29. ... After three recycles, catalysts were calcined at 550 °C for 6 h to eliminate the coke deposition and then reused to investigate the catalytic activity. ...