Journal of Crystal Growth 2018-03-29

An analysis of the specificity of defects embedded into (1 0 0) and (1 1 1) faceted CVD diamond microcrystals grown on Si and Mo substrates by using E/H field discharge

Iurii Nasieka, Victor Strelchuk, Victor Naseka, Yuriy Stubrov, Stanislav Dudnik, Vasiliy Gritsina, Oleg Opalev, Konstantin Koshevoy, Vladimir Strel'nitskij, Vasyl Tkach, Mykola Boyko, Ievgen Antypov

Index: 10.1016/j.jcrysgro.2018.03.045

Full Text: HTML

Abstract

The PE CVD method with magnetic field discharge stabilization was applied for the growth of arrays of freestanding diamond grains (island films) as well as continuous films on Mo and Si substrates with (1 1 1) and (1 0 0) faceted microcrystals, respectively. Raman, SEM, XRD and PL methods were used for search of the specific features of defects embedded into (1 0 0) and (1 1 1) faceted grains. The main characteristic differences in the defect states of the diamond island films grown on Si and Mo substrates with (1 0 0) and (1 1 1) faceted diamond microcrystals were discussed on the base of the experimental data.